Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 21.3 MPa @Thickness 2.00 mm, Temperature 23.0 °C |
3090 psi @Thickness 0.0787 in, Temperature 73.4 °F |
Type 2, 200 mm/min Across Flow; ISO 37 |
PolyOne OnFlex™ U 5470A-E0083 Thermoplastic Elastomer (TPE) OnFlex™-U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™-U 5400 series are based upon alloys of SEBS and aliphatic TPU, combining the adv.. |