Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 14.1 MPa @Treatment Temp. 25.0 °C, Time 259000 sec |
2050 psi @Treatment Temp. 77.0 °F, Time 72.0 hour |
Aged fuel C |
LG Chemical NBR 6250 High Acrylonitrile Polymer Description: NBR 6250 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6250 is a non staining, medium mooney, an.. |