Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 13.0 MPa @Temperature 21.0 °C |
1890 psi @Temperature 69.8 °F |
Die C Flow 2 hr; ASTM D412 |
PolyOne Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Tensile Strength at Break | 13.0 MPa @Temperature 60.0 °C |
1890 psi @Temperature 140 °F |
|
LATI Latene® 7H2W TR/40 PP Homopolymer, Mineral Reinforced, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |