Mechanical Properties Metric English Comments
Tensile Strength at Break 17.7 MPa

@Thickness 2.00 mm,
Temperature 23.0 °C
2570 psi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type 2, 200 mm/min Across Flow; ISO 37
PolyOne OnFlex™ U 5370A-E0077 Thermoplastic Elastomer (TPE)
OnFlex™ U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™ U 5300 series are based upon alloys of SEBS and TPU, combining the advantages of..
Tensile Strength at Break 17.7 MPa

@Thickness 2.00 mm,
Temperature 23.0 °C
2570 psi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type 2, 200 mm/min; Flow; ISO 37
PolyOne OnFlex™ U 5370A-E0077 Thermoplastic Elastomer (TPE)
OnFlex™ U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™ U 5300 series are based upon alloys of SEBS and TPU, combining the advantages of..
Tensile Strength at Break 17.7 MPa

@Temperature 150 °C,
Time 1190 sec
2570 psi

@Temperature 302 °F,
Time 0.330 hour
Cured
LG Chemical NBR 3250 High Acrylonitrile Polymer
Description: NBR 3250 is a copolymer of butadiene and acrylonitrile manufactured by cold emulsion polymerization technology of Goodyear Tire and Rubber Company, USA. NBR 3250 is a non staining, medi..