Mechanical Properties Metric English Comments
Tensile Strength at Break 979 MPa

@Temperature 649 °C
142000 psi

@Temperature 1200 °F
Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy
The newest of the high-performance superalloys invented by Special Metals Corporation, INCONEL® alloy 783 (UNS R30783/US Patent 5,478,417), is an oxidation-resistant, low expansion, nickel-cobalt..