Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 960 MPa @Temperature 20.0 °C |
139000 psi @Temperature 68.0 °F |
Plate; Transverse |
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL.. |