Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 700 - 890 MPa @Thickness 65.0 mm |
102000 - 129000 psi @Thickness 2.56 in |
|
ThyssenKrupp N-A-XTRA® M 620 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Tensile Strength at Break | 700 - 890 MPa @Thickness >=65.0 mm |
102000 - 129000 psi @Thickness >=2.56 in |
|
ThyssenKrupp N-A-XTRA® M 620 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |