Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1250 MPa @Temperature 400 °C |
181000 psi @Temperature 752 °F |
|
Special Metals UDIMET® alloy 520 Superalloy UDIMET® alloy 520 is a precipitation-hardenable nickel base superalloy with an exceptional combination of high-temperature mechanical properties, corrosion resistance and forgeability characteris.. |