Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1126 MPa @Temperature 200 °C |
163300 psi @Temperature 392 °F |
|
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium .. |