Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 75.8 MPa @Temperature 175 °C |
11000 psi @Temperature 347 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Tensile Strength at Break | 75.8 MPa @Temperature 175 °C |
11000 psi @Temperature 347 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Tensile Strength at Break | 75.8 MPa @Temperature 23.9 °C |
11000 psi @Temperature 75.0 °F |
|
Master Bond EP46HT Epoxy Adhesive for Structural Bonding Description: Master Bond System EP46HT is a newly formulated two component high performance heat resistant epoxy resin system with excellent mechanical strength and chemically resistant properties f.. |
|||
Tensile Strength at Break | 76.0 MPa @Temperature 23.0 °C |
11000 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Minlon® EFE6096 GY090A Nylon 66
(Unverified Data**) Minlon® EFE6096 GY090A is a 15% mineral reinforced impact modified nylon 66 resin.Information provided by DuPont Performance Polymers |