Tensile Strength at Break >= 103 MPa

@Temperature 300 °C
>= 14900 psi

@Temperature 572 °F
PEAK Werkstoff DISPAL S250 Aluminum Alloy, AlSi20Fe5Ni2, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Tensile Strength at Break 103 MPa

@Temperature 23.0 °C
14900 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66
Information provided by DuPont Performance Polymers