Tensile Strength at Break >= 68.9 MPa

@Temperature 23.9 °C
>= 10000 psi

@Temperature 75.0 °F
Master Bond EP112M Two Component, Medium Viscosity Heat Curing Cycloaliphatic Epoxy Resin
Product Description: Master Bond Polymer System EP112M is a solventless, medium viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor ..