Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 10.5 MPa @Thickness 2.00 mm, Temperature 23.0 °C |
1520 psi @Thickness 0.0787 in, Temperature 73.4 °F |
200 mm/min Across Flow; DIN 53504 |
PolyOne OnFlex™ HT 60A-3S2101 Thermoplastic Elastomer (TPE) OnFlex™ HT thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds is specially formulated to deliver very good compression set performance at.. |