Polymer Property : Tensile Strength at Break = 1.38 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.38 MPa

@Temperature 60.0 °C,
Time 1.21e+6 sec
200 psi

@Temperature 140 °F,
Time 336 hour
JRF; AMS-S83318
3M AC-250 B-1/6 Aerospace Sealant
3M Aerospace Sealant AC-250 B-1/6 is a two-part, polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a thixotropic paste and can be read..