Mechanical Properties Metric English Comments
Tensile Strength at Break 0.186 MPa

@Temperature 93.0 °C
27.0 psi

@Temperature 199 °F
Flatwise, high pressure laminate/particle board, test speed 0.05 in/min
3M Fastbond™ 30-NF Contact Adhesive
3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M
Tensile Strength at Break 0.186 MPa

@Temperature 93.0 °C
27.0 psi

@Temperature 199 °F
Flatwise, high pressure laminate/particle board, test speed 0.05 in/min
3M Fastbond™ 30H-NF Contact Adhesive
3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M