Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 0.0700 MPa @Temperature 175 °C |
10.2 psi @Temperature 347 °F |
T-Block on Aluminum; ASTM D987 |
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Tensile Strength at Break | 0.0700 MPa @Temperature 230 °C |
10.2 psi @Temperature 446 °F |
T-Block on Aluminum; ASTM D987 |
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Tensile Strength at Break | 0.0700 MPa @Temperature 175 °C |
10.2 psi @Temperature 347 °F |
T-Block on Aluminum; ASTM D987 |
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Tensile Strength at Break | 0.0700 MPa @Temperature 230 °C |
10.2 psi @Temperature 446 °F |
T-Block on Aluminum; ASTM D987 |
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Tensile Strength at Break | 0.0700 MPa @Temperature 107 °C |
10.2 psi @Temperature 225 °F |
T-Block on Aluminum; ASTM D987 |
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Tensile Strength at Break | 0.0700 MPa @Temperature 150 °C |
10.2 psi @Temperature 302 °F |
T-Block on Aluminum; ASTM D987 |
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Tensile Strength at Break | 0.0700 MPa @Temperature 175 °C |
10.2 psi @Temperature 347 °F |
T-Block on Aluminum; ASTM D987 |
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Tensile Strength at Break | 0.0700 MPa @Temperature 107 °C |
10.2 psi @Temperature 225 °F |
T-Block on Aluminum; ASTM D987 |
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Tensile Strength at Break | 0.0700 MPa @Temperature 150 °C |
10.2 psi @Temperature 302 °F |
T-Block on Aluminum; ASTM D987 |
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Tensile Strength at Break | 0.0700 MPa @Temperature 175 °C |
10.2 psi @Temperature 347 °F |
T-Block on Aluminum; ASTM D987 |
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |