Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 11.5 kJ/m² @Temperature 23.0 °C |
5.47 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Eastman Spectar® 14471 Copolyester Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use .. |