Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 100 kJ/m² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
conditioned; ISO 180-1A |
Lanxess Durethan® BC 550 DUSXBL 900116 Nylon 6 PA 6, non-reinforced, extrusion, Blastorm, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 100 kJ/m² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1A |
Lanxess Durethan® TP 142-011 900116 Nylon 6 PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |