Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 36.0 kJ/m² @Temperature 23.0 °C |
17.1 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² @Temperature 23.0 °C |
17.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styrolution Terluran® SP-6 ABS Description: High impact grade, suitable for extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Izod Impact, Notched (ISO) | 36.0 kJ/m² @Temperature -20.0 °C |
17.1 ft-lb/in² @Temperature -4.00 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® ST811HS BK038 Nylon 6
(Unverified Data**) Zytel® ST811HS BK038 is a flexible, non-plasticized, black Super Tough nylon 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores an.. |