Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 32.8 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 69.0 kJ/m²

@Temperature 23.0 °C
32.8 ft-lb/in²

@Temperature 73.4 °F
ASTM D256
Styron PULSEâ„¢ 6000 BG PC/ABS Engineering Resin
Overview: PULSE 6000 BG is a PC/ABS resin offering an interesting combination of heat ageing characteristics, low temperature impact performance and high melt strength. Its low MFR enables manufactu..