Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.80 kJ/m² @Temperature 23.0 °C |
1.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-3260 55% Chalk-Filled Polypropylene Homopolymer INNOPOL® CS 1-3260 is a 55% chalk-filled polypropylene homopolymer compound /PP-H KD55 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 1-3260 is developed f.. |
|||
Izod Impact, Notched (ISO) | 3.80 kJ/m² @Temperature 23.0 °C |
1.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
LyondellBasell Hostacomâ„¢ TKS709D Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ TKS709D medium high melt flow, 1,600 MPa flexural modulus, UV-stabilized, thermoplastic elastomeric olefin (TEO) resin has an excellent combination of properties and proc.. |
|||
Izod Impact, Notched (ISO) | 3.80 kJ/m² @Temperature -30.0 °C |
1.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Styron INSPIREâ„¢ DTF8000 ES Compounded Polypropylene Overview: INSPIREâ„¢ TF 8000 ES is a superior scratch and mar resistant low gloss talc filled interior grad TPO exhibiting excellent low temperature ductility, high modulus and heat performance.M.. |