Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 7.50 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
3.57 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180/1A |
Polimeri Europa Edistir RT 461F Polystyrene High impact, heat resistant polystyrene with good stiffness. Recommended for improving the thermal performance of injection moulded technical parts which are submitted to high temperature in service.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² @Temperature 23.0 °C |
3.57 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66
(Unverified Data**) Zytel® 79G13HSL BK039 is a 13 % glass reinforced, heat stabilized, lubricated slightly toughened black polyamide 66 for injection molding. It has improved impact resistance.Information provided by .. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² @Temperature -18.0 °C |
3.57 ft-lb/in² @Temperature -0.400 °F |
ISO 180 |
LyondellBasell Pro-faxâ„¢ SG899 Polypropylene Copolymer Description: Pro-faxâ„¢ SG899 high flow, high impact polypropylene copolymer resin is tailored for use in automotive interior head impact applications. This resin is designed to be run in convent.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² @Temperature -30.0 °C |
3.57 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 180-1A |
Lanxess Durethan® B 31 FCS 000000 Nylon 6, Film Grade PA 6, non-reinforced, extrusion, low viscosity, slip agentInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² @Temperature -30.0 °C |
3.57 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 180-1A |
Lanxess Durethan® B 35 F 000000 Nylon 6, Extrusion, Low Viscosity PA 6, non-reinforced, extrusion, low viscosity, no additivesInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² @Temperature -30.0 °C |
3.57 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Sax Polymers SAXAMID 226F6RY01 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6RY01 is a polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² @Temperature 23.0 °C |
3.57 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Total PPC 10641 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 10641 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10641 is characterized by high fluidity with good mechanical prope.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² @Temperature 23.0 °C |
3.57 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Total PPC 10642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 10642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10642 is characterized by high fluidity with good mechanical prope.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² @Temperature 23.0 °C |
3.57 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Total PPC 13812 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 13812 is a high fluidity heterophasic copolymer resin with fast nucleation.Polypropylene PPC 13812 is characterized by good stiffness and impact resistance as well as low shrinkage.. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² @Temperature -30.0 °C |
3.57 ft-lb/in² @Temperature -22.0 °F |
conditioned; ISO 180/1A |
EMS-Grivory Grivory® R 47 HW 10 PA6 Grilon R 47 HW 10 is a flexible, cold impact resistant and heat stabilized polyamide 6 for applications in the extrusion. The material can be processed on all for polyamides suitable tube-extrusion .. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² @Temperature 23.0 °C |
3.57 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Domo 2300L Polypropylene Copolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² @Temperature 23.0 °C |
3.57 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Domo 2348M Polypropylene Copolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 7.50 kJ/m² @Temperature 23.0 °C |
3.57 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultrason® E 3010 MR UN PESU Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat.. |