Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 7.30 kJ/m²

@Temperature -40.0 °C
3.47 ft-lb/in²

@Temperature -40.0 °F
ISO 180/1A
NOVA Chemicals Dylark® 378P12 Glass Reinforced Engineering Resin
Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim
Izod Impact, Notched (ISO) 7.30 kJ/m²

@Thickness 4.00 mm,
Temperature -30.0 °C
3.47 ft-lb/in²

@Thickness 0.157 in,
Temperature -22.0 °F
ISO 180/1A
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade
Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®..