Izod Impact, Notched (ISO) 54.0 kJ/m²

@Temperature 23.0 °C
25.7 ft-lb/in²

@Temperature 73.4 °F
ISO 180
LyondellBasell Hifaxâ„¢ ETA3081HS Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ ETA3081HS medium melt flow, 800 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has balanced physical properties, moldability and paintability. ..
Izod Impact, Notched (ISO) 54.0 kJ/m²

@Temperature 23.0 °C
25.7 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® CL200 PBT+PC (Europe-Africa-Middle East)
XENOY CL200 is a semi-crystalline thermoplastic blend, specially developed to obtain good low temperature impact strength combined with excellent chemical resistance to occasional solvent and gasoli..