Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 2.80 kJ/m²

@Temperature -40.0 °C
1.33 ft-lb/in²

@Temperature -40.0 °F
ISO 180
LyondellBasell Hostacomâ„¢ CB189FC/1 Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ CB189FC/1 medium melt flow, 1,300 MPa flexural modulus, precolored, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of impact, stiffne..
Izod Impact, Notched (ISO) 2.80 kJ/m²

@Temperature -30.0 °C
1.33 ft-lb/in²

@Temperature -22.0 °F
ISO 180/A
Styrolution Styrolux® 693 D SBC
Description: Styrolux® 693 D is a clear styrene-butadiene copolymer (SBC) with a well balanced combination of toughness and clarity. Styrolux® 693 D is mainly used for thermoformed articles, e..
Izod Impact, Notched (ISO) 2.80 kJ/m²

@Temperature -20.0 °C
1.33 ft-lb/in²

@Temperature -4.00 °F
ISO 180/1A
Borealis Daplen™ EF341AE Polypropylene TPO Compound
Daplen™ EF341AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q..
Izod Impact, Notched (ISO) 2.80 kJ/m²

@Temperature -30.0 °C
1.33 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Domo 2340RC Polypropylene Copolymer
Information provided by Domo.