Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 2.70 kJ/m²

@Temperature 10.0 °C
1.28 ft-lb/in²

@Temperature 50.0 °F
ISO 180
LyondellBasell Hostacomâ„¢ BC142/1AC Polypropylene Copolymer
Description: Hostacomâ„¢ BC142/1AC conventional melt flow, 3,600 MPa flexural modulus, precolored, mineral-filled polypropylene copolymer has a good balance of stiffness and impact resistance. It..