Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 1.30 kJ/m² @Temperature -30.0 °C |
0.619 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Domo 1040RC Polypropylene Homopolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 1.30 kJ/m² @Temperature -30.0 °C |
0.619 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Domo 1100N Polypropylene Homopolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 1.30 kJ/m² @Temperature -30.0 °C |
0.619 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Domo 1040N Polypropylene Homopolymer Information provided by Domo. |
|||
Izod Impact, Notched (ISO) | 1.30 kJ/m² @Temperature -30.0 °C |
0.619 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Domo 1100L Polypropylene Homopolymer Information provided by Domo. |