Four Ball Wear 0.650 mm
0.0256 in
Scar mm @ 40 kg.; ASTM D-2596
ConocoPhillips Tacna® M5 Grease NLGI Grade 0
Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined..
Four Ball Wear 0.650 mm
0.0256 in
Scar mm @ 40 kg.; ASTM D-2596
ConocoPhillips Tacna® M5 Grease NLGI Grade 1
Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined..
Four Ball Wear 0.650 mm
0.0256 in
Scar mm @ 40 kg.; ASTM D-2596
ConocoPhillips Tacna® M5 Grease NLGI Grade 2
Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined..