Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Wear | 0.530 mm | 0.0209 in | 40 kg, 75°C, 1200 rpm; ASTM D4172 |
ExxonMobil Mobil Aero HFS Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |
|||
Four Ball Wear | 0.530 mm | 0.0209 in | |
ChevronTexaco NLGI 1 Moly MAX Grease EP FeaturesChevron Moly MAX Greases EP are high performance greases.They are formulated with extreme pressure additives and 5% molybdenum disulfide (moly). They are dark gray/black in color and smooth .. |
|||
Four Ball Wear | 0.530 mm | 0.0209 in | 40 kg, 75°C, 1200 rpm; ASTM D4172 |
ExxonMobil Mobil Aero HFS Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |