Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Four Ball Wear = 0.390 mm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Four Ball Wear 0.390 mm
0.0154 in
ASTM D4172
ConocoPhillips Syncon® 150 Synthetic EP Gear Oil, AGMA No. 4EP
Syncon EP Plus Gear Oil is a premium quality, synthetic, extreme-pressure industrial gear lubricant developed for the lubrication of enclosed gear drives and heavily loaded plain or rolling-element ..
Four Ball Wear 0.390 mm
0.0154 in
Non-Seizure Load, Scar; ASTM D2596, DIN 51 350
Chesterton 787 Sliding Paste
Description: Chesterton® 787 Sliding Paste is a premium quality pure synthetic lubricant that will function affectivity even at ultra high temperatures and pressures. Designed for the most severe o..
Four Ball Wear 0.390 mm
0.0154 in
Scar Diameter; ASTM D4172
ELM® 80W90 Multi-Purpose Biodegradable – Biobased Gear Lubricant
Description: ELM 80W90 Multi-Purpose Gear Lubricant is a premium quality biodegradable gear lubricant formulated with the best optimized Biotechbased™ USA-grown natural seed oil that surpasses the ..
Four Ball Wear 0.390 mm
0.0154 in
ConocoPhillips EP Conolith® Grease NLGI NO. 1
Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th..
Four Ball Wear 0.390 mm
0.0154 in
ConocoPhillips EP Conolith® Grease NLGI NO. 2
Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th..
Copyright © lookpolymers.com All Rights Reserved