Mechanical Properties Metric English Comments
Four Ball Wear 1.10 mm
0.0433 in
Avg. scar diameter; ASTM D4172
Solvay Specialty Polymers FOMBLIN® W800 PFPE Lubricant
Fomblin® PFPE fluorinated lubricants are used when harsh chemical environments, high temperatures or wide working-temperature ranges are encountered.Information provided by Solvay Solexis, Inc.