Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Wear | 0.580 mm | 0.0228 in | |
ELM® TempFlex™ 0 to 100 Biodegradable Rail Curve Lubricant Description: TempFlex™ 0 to 100 is a premium quality biodegradable, Biotechbased™ Rail Curve Lubricant formulated from USA-grown vegetable oils and a lithiumbased thickener.Applications: Designed .. |