Polymer Property : Four Ball Wear = 0.0130 in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Four Ball Wear 0.330 mm
0.0130 in
Scar Diameter; ASTM D4172
ConocoPhillips Syncon® 100 Synthetic R&O Oil
Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv..
Four Ball Wear 0.330 mm
0.0130 in
Scar Diameter; ASTM D4172
ConocoPhillips Syncon® 320 Synthetic EP Gear Oil, AGMA No. 6EP
Syncon EP Plus Gear Oil is a premium quality, synthetic, extreme-pressure industrial gear lubricant developed for the lubrication of enclosed gear drives and heavily loaded plain or rolling-element ..
Four Ball Wear 0.330 mm
0.0130 in
Scar Diameter; ASTM D4172
ConocoPhillips Syncon® 46 Synthetic R&O Oil
Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv..
Four Ball Wear 0.330 mm
0.0130 in
Scar Diameter; ASTM D4172
ConocoPhillips Syncon® 460 Synthetic EP Gear Oil, AGMA No. 7EP
Syncon EP Plus Gear Oil is a premium quality, synthetic, extreme-pressure industrial gear lubricant developed for the lubrication of enclosed gear drives and heavily loaded plain or rolling-element ..
Four Ball Wear 0.330 mm
0.0130 in
Scar Diameter; ASTM D4172
ConocoPhillips Syncon® 680 Synthetic EP Gear Oil, AGMA No. 8EP
Description: Conoco Syncon Synthetic EP Gear Oil is a synthetic polyalphaolefin (PAO) lubricant for enclosed gear sets requiring extreme-pressure gear oils and operating at high temperatures. It is ..
Four Ball Wear 0.330 mm
0.0130 in
Scar Diameter, 1800 rpm, 20 kg; ASTM D4172
ChevronTexaco Cetus® PAO 43
Texaco Cetus PAO oils deliver value through:Long lubricant life in high temperature operations — Outstanding thermal and oxidation stability.Extended machinery life and increased compressor efficie..