Polymer Property : Four Ball Wear = 0.00394 in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Four Ball Wear 0.100 mm

@Temperature 260 °C
0.00394 in

@Temperature 500 °F
Coefficient of Friction, Modified for High Heat; ASTM D 226, DIN 51 350
Chesterton 787 Sliding Paste
Description: Chesterton® 787 Sliding Paste is a premium quality pure synthetic lubricant that will function affectivity even at ultra high temperatures and pressures. Designed for the most severe o..