Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 152.9 kg
337.1 lb (mass)
Dow Corning MOLYKOTE® 41 HIGH TEMPERATURE BEARING GREASE
Phenyl-methyl silicone grease thickened with carbon blackInformation provided by Dow Corning
Four Ball Extreme Pressure, Weld Load 152.9 kg
337.1 lb (mass)
Dow Corning MOLYKOTE® G-2001
Lithium thickened bearing grease based on synthetic hydrocarbonInformation provided by Dow Corning