Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Extreme Pressure, Weld Load | 122.3 kg | 269.7 lb (mass) | |
Dow Corning MOLYKOTE® 33 EXTREME LOW TEMPERATURE BEARING GREASE, LIGHT Phenyl-methyl silicone grease for extreme low temperaturesInformation provided by Dow Corning |
|||
Four Ball Extreme Pressure, Weld Load | 122.3 kg | 269.7 lb (mass) | |
Dow Corning MOLYKOTE® 33 EXTREME LOW TEMPERATURE BEARING GREASE, MEDIUM Phenyl-methyl silicone grease for extreme low temperaturesInformation provided by Dow Corning |