Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 600 kg
1320 lb (mass)
ELM® SoyGrease™ Biodegradable Grease for Semi-Truck Fifth Wheels
Description: Elm SoyGrease™ Semi-Truck Fifth Wheel is formulated with the bestoptimized Biotechbased™ USA-grown natural seed oil that surpasses the lubricity of most conventional oils. This bi..
Four Ball Extreme Pressure, Weld Load 600 kg
1320 lb (mass)
ELM® SoyGrease™ EP Plus Biodegradable Extreme Pressure Grease, NLGI Grade 2
Description: ELM SoyGrease™ EP Plus grease is a premium quality biodegradable, Biotechbased™ grease formulated with OptiBase™ Oils, lithium-based thickener and extreme pressure additives for ma..
Four Ball Extreme Pressure, Weld Load 600 kg
1320 lb (mass)
ELM® SoyGrease™ EP Plus Biodegradable Extreme Pressure Grease, NLGI Grade 3
Description: ELM SoyGrease™ EP Plus grease is a premium quality biodegradable, Biotechbased™ grease formulated with OptiBase™ Oils, lithium-based thickener and extreme pressure additives for ma..
Four Ball Extreme Pressure, Weld Load 600 kg
1320 lb (mass)
ELM® SoyGrease™ HiTemp Biodegradable Extreme Pressure Grease, NLGI Grade 3
Description: ELM SoyGrease™ HiTemp grease is a premium quality biodegradable, Biotechbased™ grease formulated with OptiBase™ Oils, lithium-based thickener and extreme pressure additives for maxim..