Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 9.00 - 94.0 kJ/m² | 4.28 - 44.7 ft-lb/in² | Average value: 54.4 kJ/m² Grade Count:13 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |