Polymer Property : Izod Impact, Notched (ISO) = 9.28 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 19.5 kJ/m²
9.28 ft-lb/in²
Lushan PA+30% GF+5% AR-1A Nylon Toughener/PA Impact Modifier
Nylon toughener/PA impact modifier Lushan series is a maleic anhydride grafted polyolefin elastomer, with a very low residual maleic anhydride monomer, no irritating odor when using. Nylon toughener..
Copyright © lookpolymers.com All Rights Reserved