Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 6.00 - 9.20 kJ/m²
2.86 - 4.38 ft-lb/in²
Average value: 8.40 kJ/m² Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..