Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 2.00 - 80.1 kJ/m² | 0.952 - 38.1 ft-lb/in² | Average value: 30.8 kJ/m² Grade Count:14 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |