Polymer Property : Izod Impact, Notched (ISO) = 8.90 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 8.90 kJ/m²
4.24 ft-lb/in²
ISO 180-1A
Gromax BFG20-FN00N1 Nylon 6 20% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Izod Impact, Notched (ISO) 8.90 kJ/m²
4.24 ft-lb/in²
Volume Resistivity 2.5 [log(ohm-cm)]
TIMCAL ENSACO™ 250G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..