Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 7.56 kJ/m² | 3.60 ft-lb/in² | at -30C; ASTM D256; ASTM D-256 |
Ineos A60-70-162 HDPE Ineos A60-70-162 is a high density polyethylene homopolymer, developed specifically for blow molding food containers on reciprocating screw-type equipment. It exhibits excellent processing character.. |
|||
Izod Impact, Notched (ISO) | 7.56 kJ/m² | 3.60 ft-lb/in² | ISO 180/1A |
ExxonMobil PP7033L1 Polypropylene Impact Copolymer Product Description: An impact copolymer resin characterized with low flow. It is suitable for extrusion applications like sheet and thermoforming. It is also suitable for molding applications like.. |