Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 14.7 - 14.7 kJ/m² @Temperature -30.0 - -30.0 °C |
6.99 - 6.99 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 14.7 kJ/m² Grade Count:1 |
Overview of materials for Polyphenylene Ether, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Impact Grade". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched (ISO) | 14.7 kJ/m² | 6.99 ft-lb/in² | ISO 180-1A |