Polymer Property : Izod Impact, Notched (ISO) = 47.6 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 100 kJ/m²
47.6 ft-lb/in²
15°V; ISO 179
Polikim ULPOLEN® 1000 UHMWPE, Flame Retardant
For those producing flammable materials and in the mining industry, explosion and fire are major dangers. It is of vital importance that in conveyor belts and bunkers, lining material is flame retar..
Izod Impact, Notched (ISO) 100 kJ/m²
47.6 ft-lb/in²
15°V; ISO 179
Polikim ULPOLEN® 1000 UHMWPE, UV, Antistatic
In tough operating conditions and under direct sunlight, standard Ulpolen® 1000 shows signs of wear and abrasion within a period shorter than a year. It accumulates static electric during daily use..
Izod Impact, Notched (ISO) >= 100 kJ/m²
>= 47.6 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® NX07331 PC+ABS (Asia Pacific)
FARADEX NX07331 is a commercial grade EMI shielding material
Izod Impact, Notched (ISO) >= 100 kJ/m²
>= 47.6 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics LNP FARADEX NX07331 PC+ABS (Asia Pacific)
FARADEX NX07331 is a commercial grade EMI shielding material
Izod Impact, Notched (ISO) 100 kJ/m²
47.6 ft-lb/in²
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)  (Unverified Data**)
50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve..