Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 4.1202 kJ/m² | 1.9609 ft-lb/in² | ASTM D256 |
Daelim H&L Plavis G40 Aromatic Polyimide, 40% Graphite Filled, Direct Formed
(Unverified Data**) Information provided by Daelim H&L |