Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.93 kJ/m² | 1.87 ft-lb/in² | ASTM D256 |
GEHR Plastics Ultem 2300 PEI-30 GF 30% Glass Fiber Reinforced
(discontinued **) Polyetherimide has a high mechanical strength in connection with a good chemical and heat resistance, good dimensional stability and great resistance. It's unique torque strength permits the econom.. |