Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.50 - 3.50 kJ/m² @Temperature -30.0 - -30.0 °C |
1.67 - 1.67 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 3.50 kJ/m² Grade Count:1 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |