Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 7.20 kJ/m²
3.43 ft-lb/in²
Type A; ISO 180:2000
Nylacast POM C Acetal Copolymer
The copolymer grade is the ideal combination of strength, stiffness and wears resistance. It absorbs very little moisture, is easily machinable and is genuinely porosity-free making it the preferred..
Izod Impact, Notched (ISO) 7.20 - 8.95 kJ/m²
3.43 - 4.26 ft-lb/in²
Average value: 8.05 kJ/m² Grade Count:5
Overview of materials for Polycarbonate, Carbon + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu..
Izod Impact, Notched (ISO) 7.20 kJ/m²
3.43 ft-lb/in²
Sample Type A; ISO 180:2000
Global EPP POM C Acetal Copolymer
Polyacetals are highly crystalline thermoplastics, characterised by their high mechanical strength, rigidity and impact resistance. Acetal absorbs very little moisture, enabling the product to maint..
Izod Impact, Notched (ISO) 7.20 kJ/m²
3.43 ft-lb/in²
Type 1, Notch A; ISO 180
Solvay Specialty Polymers Amodel® AE-8930 Polyphthalamide (PPA), 30% Glass Fiber
Amodel® AE-8930 is a 30% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep ..
Izod Impact, Notched (ISO) 7.20 kJ/m²
3.43 ft-lb/in²
ISO 180
Solvay Specialty Polymers Amodel® DW-1130 Polyphthalamide (PPA), 30% Glass Fiber
Amodel® DW-1130 is a 30% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o..
Izod Impact, Notched (ISO) 7.20 kJ/m²
3.43 ft-lb/in²
GB/T 1843-2008
Sichuan Deyang Haton® hCF41 Polyphenylene Sulfide
Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD
Izod Impact, Notched (ISO) 7.20 kJ/m²
3.43 ft-lb/in²
ISO 180
Polyram RamSter PF321G3 PBT, 15% Glass Fiber, Flame Retardant
15% Glass fiber reinforced, flame retardant PBT for injection molding applications.Information provided by Polyram.