Izod Impact, Notched (ISO) 4.80 - 6.30 kJ/m²

@Temperature -40.0 - -40.0 °C
2.28 - 3.00 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 5.44 kJ/m² Grade Count:7
Overview of materials for PCTG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Izod Impact, Notched (ISO) 3.00 - 6.30 kJ/m²
1.43 - 3.00 ft-lb/in²
Average value: 4.95 kJ/m² Grade Count:6
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..